Stress Corrosion Cracking of Nickel Based Alloys in Water-cooled Nuclear Reactors

Stress Corrosion Cracking of Nickel Based Alloys in Water-cooled Nuclear Reactors
Author :
Publisher : Woodhead Publishing
Total Pages : 386
Release :
ISBN-10 : 9780081000625
ISBN-13 : 0081000626
Rating : 4/5 (626 Downloads)

Book Synopsis Stress Corrosion Cracking of Nickel Based Alloys in Water-cooled Nuclear Reactors by : Damien Feron

Download or read book Stress Corrosion Cracking of Nickel Based Alloys in Water-cooled Nuclear Reactors written by Damien Feron and published by Woodhead Publishing. This book was released on 2016-01-30 with total page 386 pages. Available in PDF, EPUB and Kindle. Book excerpt: Stress Corrosion Cracking of Nickel Based Alloys in Water-Cooled Nuclear Reactors: The Coriou Effect presents the latest information on brittle failure of metals in corrosive chemical environments under the influence of tensile stresses. Nickel alloys are more resistant to SCC as well as high temperatures and have been widely used in more challenging environments such as nuclear power plants. However, these alloys can suffer SCC under certain conditions, resulting in component failure. A key figure in understanding the mechanisms of SCC in nickel alloys in water-cooled nuclear reactors is Henri Coriou of the CEA, France's leading center for nuclear research. This book assesses his work in the context of the latest research on SCC in nickel alloys in nuclear power plants. - Up-to-date reviews of recent research findings from leading experts in the field - Authoritative and comprehensively reviewed by the Working Party 4 on Nuclear Corrosion - Showcases the excellent quality and technical accomplishments of Henri Coriou and CEA


Stress Corrosion Cracking of Nickel Based Alloys in Water-cooled Nuclear Reactors Related Books

Stress Corrosion Cracking of Nickel Based Alloys in Water-cooled Nuclear Reactors
Language: en
Pages: 386
Authors: Damien Feron
Categories: Technology & Engineering
Type: BOOK - Published: 2016-01-30 - Publisher: Woodhead Publishing

GET EBOOK

Stress Corrosion Cracking of Nickel Based Alloys in Water-Cooled Nuclear Reactors: The Coriou Effect presents the latest information on brittle failure of metal
Structural Alloys for Nuclear Energy Applications
Language: en
Pages: 676
Authors: Robert Odette
Categories: Technology & Engineering
Type: BOOK - Published: 2019-08-15 - Publisher: Newnes

GET EBOOK

High-performance alloys that can withstand operation in hazardous nuclear environments are critical to presentday in-service reactor support and maintenance and
Nuclear Corrosion
Language: en
Pages: 496
Authors: Stefan Ritter
Categories: Technology & Engineering
Type: BOOK - Published: 2020-08-15 - Publisher: Woodhead Publishing

GET EBOOK

Nuclear Corrosion: Research, Progress and Challenges, part of the "Green Book” series of the EFC, builds upon the foundations of the very first book published
Nuclear Science Abstracts
Language: en
Pages: 680
Authors:
Categories: Nuclear energy
Type: BOOK - Published: 1976 - Publisher:

GET EBOOK

MECHANICAL ENGINEERING, ENERGY SYSTEMS AND SUSTAINABLE DEVELOPMENT -Volume III
Language: en
Pages: 504
Authors: Konstantin V. Frolov
Categories: Economic development
Type: BOOK - Published: 2009-04-15 - Publisher: EOLSS Publications

GET EBOOK

Mechanical Engineering, Energy Systems and Sustainable Development theme is a component of Encyclopedia of Physical Sciences, Engineering and Technology Resourc