Book Synopsis Stress-corrosion Cracking of Aluminum Alloys by : F. H. Haynie

Download or read book Stress-corrosion Cracking of Aluminum Alloys written by F. H. Haynie and published by . This book was released on 1966 with total page 52 pages. Available in PDF, EPUB and Kindle. Book excerpt: This report deals with the stress-corrosion cracking of aluminum alloys, and it represents an effort by DMIC to expand on the information contained in DMIC Memorandum 202, 'Stress-Corrosion Cracking of Aluminum Alloys', dated February 15, 1965. DMIC Report 228 begins by presenting a comprehensive definition of stress-corrosion cracking. This is followed by sections dealing with (1) the historical development and growth in awareness of the problem, (2) the mechanisms involved, and (3) the theory of stress-corrosion cracking. A section on experimental techniques is presented. These techniques include test methods used to determine the susceptibility of alloys to stress-corrosion cracking, as well as more refined methods of studying the fundamental mechanisms of the problem. Different evaluation methods, applicable to obtaining the different objectives of stress-corrosion testing, are also presented. All of the foregoing serve as background to the sections on stress-corrosion-cracking behavior of aluminum alloys and preventive measures. (Author).


Stress-corrosion Cracking of Aluminum Alloys Related Books

Stress-corrosion Cracking of Aluminum Alloys
Language: en
Pages: 52
Authors: F. H. Haynie
Categories: Aluminum alloys
Type: BOOK - Published: 1966 - Publisher:

GET EBOOK

This report deals with the stress-corrosion cracking of aluminum alloys, and it represents an effort by DMIC to expand on the information contained in DMIC Memo
Stress-corrosion Cracking
Language: en
Pages: 466
Authors: Russell H. Jones
Categories: Science
Type: BOOK - Published: 1992 - Publisher: ASM International(OH)

GET EBOOK

Details the many conditions under which stress-corrosion cracking (SCC) can occur, the parameters which control SCC, and the methodologies for mitigating and te
Corrosion of Aluminum and Aluminum Alloys
Language: en
Pages: 336
Authors: Joseph R. Davis
Categories: Technology & Engineering
Type: BOOK - Published: 1999-01-01 - Publisher: ASM International

GET EBOOK

Stress Corrosion Cracking
Language: en
Pages: 817
Authors: V S Raja
Categories: Technology & Engineering
Type: BOOK - Published: 2011-09-22 - Publisher: Elsevier

GET EBOOK

The problem of stress corrosion cracking (SCC), which causes sudden failure of metals and other materials subjected to stress in corrosive environment(s), has a
Stress-corrosion Cracking of Aluminum Alloys
Language: en
Pages: 22
Authors: J. D. Jackson
Categories: Aluminum alloys
Type: BOOK - Published: 1965 - Publisher: